| Alloy | Chemical Composition(%) | Conductivity(IACS) | |
| JIS | GB | Cu+Ag | |
| C1100 | T2 | 99.90% | 96% |
| C1020 | TU2 | 99.96% | 100% |
| Features and Use | High purity, good conductive,thermal conductivity, processability, welding performance, and good corrosion resistance.Used for heat dissipation device and electric conduction devices.etc. | ||
| JIS | TEMPER | GB | Tensile Strength(N/m2) | Elongation(%) | Hardness(HV) |
| C1100 | O | T2 | >=195 | >=35 | / |
| H/4 | T2 | 215-275 | >=25 | 55-100 | |
| H/2 | T2 | 245-315 | >=15 | 75-120 | |
| H | T2 | >=275 | / | >=80 | |
| C1020 | O | TU2 | >=195 | >=35 | / |
| H/4 | TU2 | 215-275 | >=25 | 55-100 | |
| H/2 | TU2 | 245-315 | >=15 | 75-120 | |
| H | TU2 | >=275 | / | >=80 |
| Alloy | Chemical Composition(%) | Conductivity(IACS) | |
| JIS | GB | Cu+Ag | |
| C1100 | T2 | 99.90% | 96% |
| C1020 | TU2 | 99.96% | 100% |
| Features and Use | High purity, good conductive,thermal conductivity, processability, welding performance, and good corrosion resistance.Used for heat dissipation device and electric conduction devices.etc. | ||
| JIS | TEMPER | GB | Tensile Strength(N/m2) | Elongation(%) | Hardness(HV) |
| C1100 | O | T2 | >=195 | >=35 | / |
| H/4 | T2 | 215-275 | >=25 | 55-100 | |
| H/2 | T2 | 245-315 | >=15 | 75-120 | |
| H | T2 | >=275 | / | >=80 | |
| C1020 | O | TU2 | >=195 | >=35 | / |
| H/4 | TU2 | 215-275 | >=25 | 55-100 | |
| H/2 | TU2 | 245-315 | >=15 | 75-120 | |
| H | TU2 | >=275 | / | >=80 |